Analysis of O-Ring damage

SPIRAL FAILURE

■Description

Cutting damage and spiral failure appear on the seal surface.

■Contributing factors

  • The joint line of the seal is irregular, or the surface is not flat

  • The seal is not lubricated properly during installation

  • The groove is tight

  • The seal is installed on the groove subject to parallel translation

  • The seal of poor quality or low hardness

  • The installation technique of the technician is poor

■Recommended improving method

  • Correctly install, lubricate or design the seal

  • Adopt the seal of good quality or higher hardness

  • Enhance the training to the technicians